Test Property | Unit | Test Method | Minimum Average Value (per GRI GM13) | ||||||
Thickness (1) mm | ASTM D 5199 | 0.5 | 0.75 | 1.0 | 1.5 | 2.0 | 2.5 | 3.0 | |
Lowest individual (-10%) | ASTM D 5199 | 20 | 30 | 40 | 60 | 80 | 100 | 120 | |
Density | ASTM D 792 | ≥0.94 |
|||||||
Strength at Yield (Both Directions) | ASTM D 6693 | 8 | 11 | 15 | 22 | 29 | 37 | 44 | |
Strength at Break (Both Directions) | Type IV Dumbbell, 50mm/min | 14 | 20 | 27 | 40 | 53 | 67 | 80 | |
Elongation at Yield (Both Directions) | % | Gage length 33 mm for Yield Elongation | 12 | 12 | 12 | 12 | 12 | 12 | 12 |
Elongation at Break (Both Directions) | Gage length 50 mm for break Elongation | 700 | 700 | 700 | 700 | 700 | 700 | 700 | |
Tear Resistance | N | ASTM D 1004 | 63 | 93 | 125 | 187 | 249 | 311 | 374 |
Puncture Resistance | N | ASTM D 4833 | 160 | 240 | 320 | 480 | 640 | 800 | 960 |
Carbon Black Content | % | ASTM D 1603 | 2.0% - 3.0% | ||||||
Carbon Black Dispersion | Category | ASTM D 5596 | Note (2) | ||||||
Dimensional Stability | % | ASTM D 1204 (120 ºC/ 1 h) |
± 2 | ±2 | ±2 | ±2 | ±2 | ±2 | ± 2 |
Melt Flow Index (3) | g/10 min | ASTM D 1238 (190ºC/2.16 kg) | ≤ 1 | ≤1 | ≤1 | ≤1 | ≤1 | ≤1 | ≤ 1 |
Low Temperature Brittleness | ºC | ASTM D 746 | -77 | -77 | -77 | -77 | -77 | -77 | -77 |
Stress Crack Resistance (NCTL) | hr. | ASTM D 5397 | ≥ 500 |
≥500 | ≥500 | ≥500 | ≥500 | ≥500 | ≥500 |
Oxidative Induction Time (Standard; S-OIT) | min | ASTM D 3895 | 100 | 100 | 100 | 100 | 100 | 100 | 100 |
Oxidative Induction Time (High Pressure; HP-OIT) | min | ASTM D 5885 | 400 | 400 | 400 | 400 | 400 | 400 | 400 |